    SME facilitators –
    Damon McCrory, Harbison-Walker Refractories Co & Barry Robinson, Middough
     
    Refractory Failure
    Between FGSV & orifice chamber
    At 1100-1200F on steel OD
    Failed after 1 year
    Look at process conditions, refractory type, vendor, anchors
    Dryout Temps
    300 F with hold
    600-700 F with hold
    1000- 1200 F with hold
    24 hr air cure important
    HIS: jave hydrotested lined vessels with curing afterward
    Structure tours: once every 2 hours with cold marked.